Department of Chemical Engineering, Indian Institute of Technology Guwahati, Guwahati 781039, India
G. Pugazhenthi, E-mail: pugal@iitg.ernet.in
收稿:2015-11-16,
修回:2016-1-19,
录用:2016-1-24,
纸质出版:2016-06
Scan QR Code
Chakraborty Samarshi, Kumar Manish, Suresh Kelothu, 等. Investigation of Structural, Rheological and Thermal Properties of PMMA/ONi-Al LDH Nanocomposites Synthesized
Chakraborty Samarshi, Kumar Manish, Suresh Kelothu, et al. Investigation of Structural, Rheological and Thermal Properties of PMMA/ONi-Al LDH Nanocomposites Synthesized
Chakraborty Samarshi, Kumar Manish, Suresh Kelothu, 等. Investigation of Structural, Rheological and Thermal Properties of PMMA/ONi-Al LDH Nanocomposites Synthesized
Chakraborty Samarshi, Kumar Manish, Suresh Kelothu, et al. Investigation of Structural, Rheological and Thermal Properties of PMMA/ONi-Al LDH Nanocomposites Synthesized
This article addresses the synthesis of organically tailored Ni-Al layered double hydroxide (ONi-Al LDH) and its use in the fabrication of exfoliated poly(methyl methacrylate) (PMMA) nanocomposites. The pristine Ni-Al LDH was initially synthesized by co-precipitation method and subsequently modified using sodium dodecyl sulfate to obtain ONi-Al LDH. Nanocomposites of PMMA containing various amounts of modified Ni-Al LDH (3 wt%-7 wt%) were synthesized
via
solvent blending method to investigate the influence of LDH content on the properties of PMMA matrix. Several characterization methods such as X-ray diffraction (XRD)
transmission electron microscopy (TEM)
Fourier transform infrared spectroscopy (FTIR)
rheological analysis
differential scanning calorimetry (DSC) and thermo gravimetric analysis (TGA)
were employed to examine the structural
viscoelastic and thermal properties of PMMA/OLDH nanocomposites. The results of XRD and TEM examination confirm the formation of partially exfoliated PMMA/OLDH nanocomposites. The FTIR results elucidate that the characteristic bands for both pure PMMA and modified LDH are present in the spectra of PMMA/OLDH nanocomposites. Rheological analyses were carried out to examine the adhesion between polymer matrix and fillers present in the nanocomposite sample. The TGA data indicate that the PMMA nanocomposites exhibit higher thermal stability when compared to pure PMMA. The thermal decomposition temperature of PMMA/OLDH nanocomposites increases by 28 K compared to that of pure PMMA at 15% weight loss as a point of reference. In comparison with pure PMMA
the PMMA nanocomposite containing 7 wt% LDH demonstrates improved glass transition temperature (
T
g
) of around 3 K. The activation energy (
E
a
)
reaction orders (
n
) and reaction mechanism of thermal degradation of PMMA/OLDH nanocomposites were evaluated using different kinetic models. Water uptake capacity of the PMMA/OLDH nanocomposites is less than that of the pure PMMA.
M Alexandre, , P Dubois, . Mater. Sci. Eng. . R-Rep , 2000 . 28 1 .
A. Usuki, , Y. Kojima, , M. Kawasumi, , A. Okada, , Y. Fukushima, , T. Kurauchi, , O. Kamigaito, . . J. Mater. Res. , 1993 . 8 1179 .
T Lan, , T Pinnavaia, . . Chem. Mater. , 1994 . 6 2216 .
E.P. Giannelis, . . Adv. Mater. , 1996 . 8 29 .
P.B Messersmith, , E.P. Giannelis, . . Chem. Mater. , 1994 . 6 1719 .
Y. Kojima, , K. Fukumori, , A. Usuki, , A Okada, , T. Kurauchi, . . J. Mater. Sci. Lett. , 1993 . 12 889 .
L. Wang, , X. Xie, , S. Su, , J Feng, , C.A. Wilkie, . . Polym. Degrad. Stab. , 2010 . 95 572 .
W Chen, , B. Qu, . . Chem. Mater. , 2003 . 15 3208 .
D Paul, , L. Robeson, . . Polymer , 2008 . 49 3187 .
D.Y. Wang, , A. Das, , A. Leuteritz, , R. Boldt, , L. Häußler, , U Wagenknecht, , G. Heinrich, . . Polym. Degrad. Stab. , 2011 . 96 285 .
L. Du, , B Qu, , M. Zhang, . . Polym. Degrad. Stab. , 2007 . 92 497 .
L. Qiu, , W Chen, , B. Qu, . . Colloid. Polym. Sci. , 2005 . 283 1241 .
G.A. Wang, , C.C Wang, , C.Y. Chen, . . Polym. Degrad. Stab. , 2006 . 91 2443 .
L Qiu, , B. Qu, . . J. Colloid Interface Sci. , 2006 . 301 347 .
M Huskić, , M. Žigon, . . Eur. Polym. J. , 2007 . 43 4891 .
S.V Krishna, , G. Pugazhenthi, . . J. Exp. Nanosci. , 2012 . 8 19 .
B Sahu, , G. Pugazhenthi, . . J. Appl. Polym. Sci. , 2011 . 120 2485 .
K.E Strawhecker, , E. Manias, . . Chem. Mater. , 2000 . 12 2943 .
L. Unnikrishnan, , S. Mohanty, , S.K Nayak, , A. Ali, . . Mater. Sci. Eng., A , 2011 . 528 3943 .
F Leroux, , J.P. Besse, . . Chem. Mater. , 2001 . 13 3507 .
P. Nalawade, , B. Aware, , V Kadam, , R. Hirlekar, . . J. Sci. Ind. Res. , 2009 . 68 267 .
N. Hong, , L. Song, , B. Wang, , A.A. Stec., , T.R. Hull, , J Zhan, , Y. Hu, . . Mater. Res. Bull. , 2014 . 49 657 .
M. Li., , J.E. Zhu, , L. Zhang, , X. Chen, , H. Zhang, , F. Zhang, , S Xu, , D.G. Evans, . . Nanoscale , 2011 . 3 4240 .
Y. Wimalasiri, , R. Fan, , X.S Zhao, , L. Zou, . . Electrochim. Acta , 2014 . 134 127 .
H. Zhu, , Q. Liu, , Z. Li, , J. Liu, , X. Jing, , H Zhang, , J. Wang, . . RSC Adv. , 2015 . 5 49204 .
C. Nyambo, , D. Chen, , S Su, , C.A. Wilkie, . . Polym. Degrad. Stab. , 2009 . 94 1298 .
C. Manzi-Nshuti, , D. Wang, , J.M Hossenlopp, , C.A. Wilkie, . . Polym. Degrad. Stab. , 2009 . 94 705 .
B. Li, , Y. Hu, , J. Liu, , Z Chen, , W. Fan, . . Colloid. Polym. Sci. , 2003 . 281 998 .
W Chen, , B. Qu, . . Polym. Degrad. Stab. , 2005 . 90 162 .
Z. Zhou, , S. Wang, , L. Lu, , Y Zhang, , Y. Zhang, . . Compos. Sci. Technol. , 2007 . 67 1861 .
I. Ivanov, , S. Muke, , N Kao, , S.N. Bhattacharya, . . Polymer , 2001 . 42 9809 .
M.H Al-Saleh, , U. Sundararaj, . . Composites Part A , 2011 . 42 2126 .
P Ding, , B. Qu, . . J. Colloid Interface Sci. , 2005 . 291 13 .
J.W. Gilman, , C.L. Jackson, , A.B. Morgan, , Harris , R. Jr. , E. Manias, , E. P. Giannelis, , M. Wuthenow, , D Hilton, , S.H. Philips, . . Chem. Mater. , 2002 . 12 1886 .
A. Tomar, , S Mahendia, , S. Kumar, . . Adv. Appl. Sci. Res. , 2011 . 2 65 .
A.B Morgan, , J.W. Gilman, . . J. Appl. Polym. Sci. , 2003 . 87 1329 .
S Mohanty, , S.K. Nayak, . . J. Thermoplast. Compos. , 2010 . 23 623 .
Z. Shen, , G.P Simon, , Y.B. Cheng, . . J. Appl. Polym. Sci. , 2004 . 92 2101 .
H.A. Stretz, , D.R. Paul, , R. Li, , H Keskkula, , P.E. Cassidy, . . Polymer , 2005 . 46 2621 .
A.W Coats, , J.P. Redfern, . . Nature , 1964 . 201 68 .
Y Chen, , Q. Wang, . . Polym. Degrad. Stab. , 2007 . 92 280 .
S Krishna, , G. Pugazhenthi, . . J. Appl. Polym. Sci. , 2011 . 120 1322 .
J.M. Criado, , J Málek, , A. Ortega, . . Thermochim. Acta , 1989 . 147 377 .
G.I Senum, , R.T. Yang, . . J. Therm. Anal. , 1977 . 11 445 .
J.H. Flynn, . . Thermochim. Acta , 1997 . 300 83 .
S.J. Park, , K Li, , S.K. Hong, . . J. Ind. Eng. Chem. , 2005 . 11 561 .
H.B. Zhang, , W.G. Zheng, , Q. Yan, , Z.G Jiang, , Z.Z. Yu, . . Carbon , 2012 . 50 5117 .
M. Majid , E.D. Hassan, , A. Davoud, , M. Saman, . . Composites Part B , 2011 . 42 2038 .
0
浏览量
18
Downloads
0
CSCD
关联资源
相关文章
相关作者
相关机构
京公网安备11010802046900号