Jiang-wei Zhao, Han Zhu, Yi-xian Wu, 等. EFFECTS OF CHAIN MICROSTRUCTURE OF BUTADIENE-ISOPRENE COPOLYMERS ON THEIR GLASS TRANSITION AND CRYSTALLIZATION[J]. 高分子科学(英文版), 2010,28(4):475-482.
Jiang-wei Zhao, Han Zhu, Yi-xian Wu, et al. EFFECTS OF CHAIN MICROSTRUCTURE OF BUTADIENE-ISOPRENE COPOLYMERS ON THEIR GLASS TRANSITION AND CRYSTALLIZATION[J]. 2010, 28(4): 475-482.
Jiang-wei Zhao, Han Zhu, Yi-xian Wu, 等. EFFECTS OF CHAIN MICROSTRUCTURE OF BUTADIENE-ISOPRENE COPOLYMERS ON THEIR GLASS TRANSITION AND CRYSTALLIZATION[J]. 高分子科学(英文版), 2010,28(4):475-482.DOI: 10.1007/s10118-010-9053-6.
Jiang-wei Zhao, Han Zhu, Yi-xian Wu, et al. EFFECTS OF CHAIN MICROSTRUCTURE OF BUTADIENE-ISOPRENE COPOLYMERS ON THEIR GLASS TRANSITION AND CRYSTALLIZATION[J]. 2010, 28(4): 475-482.DOI: 10.1007/s10118-010-9053-6.
EFFECTS OF CHAIN MICROSTRUCTURE OF BUTADIENE-ISOPRENE COPOLYMERS ON THEIR GLASS TRANSITION AND CRYSTALLIZATION
A series of butadiene-isoprene copolymers (BIR) with various compositions were synthesized with a neodymium-based catalyst system. The microstructure
composition and sequence of copolymers were characterized by FTIR and 13C-NMR spectroscopy. The crystallization behavior of the BIR copolymers was investigated by DSC analysis. The results demonstrate that the content of cis-1
4 configuration in both butadiene (Bd) and isoprene (Ip) units are around 98% when Bd content in feed (fBd) covering the range from 55.7 mol% to 96.0 mol%. The reactivity ratios of Bd and Ip were determined to be 1.40 and 0.48 respectively. The random copolymers of Bd and Ip show only one glass transition temperature (Tg) from -107.4°C to -80.5°C
which is dependent on the composition and fits nicely with Fox equation. The sequence distribution followed the first-order Markov statistical model. It is found that the copolymer chains with higher Bd content contain longer polybutadiene (PBd) segments
and the sequence length of PBd segments (NBd) exhibits great influence on the crystallization behavior of the copolymer. The copolymers with NBd ≥ 11.8 could crystallize at low temperatures -71°C to -43°C). The crystallization temperature and enthalpy values decreased gradually with decreasing NBd. The copolymers with NBd ≤ 7.9 are amorphous even at very low temperatures (0°C to-150°C) due to the short PBd segments.
Abstract
A series of butadiene-isoprene copolymers (BIR) with various compositions were synthesized with a neodymium-based catalyst system. The microstructure
composition and sequence of copolymers were characterized by FTIR and 13C-NMR spectroscopy. The crystallization behavior of the BIR copolymers was investigated by DSC analysis. The results demonstrate that the content of cis-1
4 configuration in both butadiene (Bd) and isoprene (Ip) units are around 98% when Bd content in feed (fBd) covering the range from 55.7 mol% to 96.0 mol%. The reactivity ratios of Bd and Ip were determined to be 1.40 and 0.48 respectively. The random copolymers of Bd and Ip show only one glass transition temperature (Tg) from -107.4°C to -80.5°C
which is dependent on the composition and fits nicely with Fox equation. The sequence distribution followed the first-order Markov statistical model. It is found that the copolymer chains with higher Bd content contain longer polybutadiene (PBd) segments
and the sequence length of PBd segments (NBd) exhibits great influence on the crystallization behavior of the copolymer. The copolymers with NBd ≥ 11.8 could crystallize at low temperatures -71°C to -43°C). The crystallization temperature and enthalpy values decreased gradually with decreasing NBd. The copolymers with NBd ≤ 7.9 are amorphous even at very low temperatures (0°C to-150°C) due to the short PBd segments.
关键词
Keywords
references
The trial reading is over, you can activate your VIP account to continue reading.
Highly Regio- and trans-Selective Ring-opening Metathesis Polymerization of Chiral Aza-norbornene with a Simple Phenylimido-Tungsten Catalyst
Special Topic: Chirality in Polymers
Upgrading Commercially Available Polyethylene to High-value Materials with Strong Mechanical Performance and Hydrophilicity by Blending with Ethylene/meta-Methoxystyrene Copolymers
Tunable Circularly Polarized Luminescence of Helical Poly(phenylacetylene)s via Side-chain-to-Backbone Förster Resonance Energy Transfer
Topology-regulated Co-assembly of Single Chain Polymer Nanoparticles and Block Copolymers into Hierarchical Micelle@Vesicle Composite Structures