ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER
Papers|Updated:2021-06-21
|
ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER
ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER
高分子科学(英文版)2005年23卷第4期 页码:363-366
Affiliations:
Author bio:
Funds:
DOI:
中图分类号:
纸质出版:2005-07-20
Accepted:
Scan QR Code
M. E. Haquea, K. Makuuchia, F. Yoshiia, 等. ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER[J]. 高分子科学(英文版), 2005,23(4):363-366.
M. E. Haquea, K. Makuuchia, F. Yoshiia, et al. ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER[J]. 2005, 23(4): 363-366.
M. E. Haquea, K. Makuuchia, F. Yoshiia, 等. ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER[J]. 高分子科学(英文版), 2005,23(4):363-366.DOI:
M. E. Haquea, K. Makuuchia, F. Yoshiia, et al. ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER[J]. 2005, 23(4): 363-366.DOI:
ROLE OF SYNTHETIC ANTIOXIDANTS ON THE AGING PROPERTY OF ELECTRON BEAM IRRADIATED NATURAL RUBBER
The aging property of radiation vulcanized natural rubber was studied using various kinds of antioxidants. Aging test was done at 100℃ for various lengths of time. It was found that some antioxidants are excellent in preventing the oxidative degradation of the irradiated rubber. DAH (2
5-di-tert-amylhydroquinone) + CBP (2
2-dihydroxy-3
3-di(-methyl-cyclohexyl)-5
5-dimethyl diphenyl methane) + P16 (tris(2
4-di-tert-butylphenyl)phosphate) in a proportion of (1:0.5:0.5) was found to be the best combination to achieve 100% retention of tensile strength.
Abstract
The aging property of radiation vulcanized natural rubber was studied using various kinds of antioxidants. Aging test was done at 100℃ for various lengths of time. It was found that some antioxidants are excellent in preventing the oxidative degradation of the irradiated rubber. DAH (2
5-di-tert-amylhydroquinone) + CBP (2
2-dihydroxy-3
3-di(-methyl-cyclohexyl)-5
5-dimethyl diphenyl methane) + P16 (tris(2
4-di-tert-butylphenyl)phosphate) in a proportion of (1:0.5:0.5) was found to be the best combination to achieve 100% retention of tensile strength.
关键词
Keywords
references
The trial reading is over, you can activate your VIP account to continue reading.