PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)*
Papers|Updated:2021-06-21
|
PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)*
PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)*
高分子科学(英文版)1991年9卷第3期 页码:238-245
Affiliations:
1. Chemical Engineering Department, Zhejiang University,Hangzhou,310027
2. Zhejiang University
3. Hangzhou 310027
Author bio:
Funds:
DOI:
中图分类号:
纸质出版:1991-09-20
Accepted:
Scan QR Code
[1]楼剑锋,翁志学,黄志明,潘祖仁.PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)[J].Chinese Journal of Polymer Science,1991,{4}(03):238-245.
LOU Jianfeng, WENG Zhixue, HUANG Zhiming, et al. PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)*[J]. 1991, 9(3): 238-245.
[1]楼剑锋,翁志学,黄志明,潘祖仁.PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)[J].Chinese Journal of Polymer Science,1991,{4}(03):238-245.DOI:
LOU Jianfeng, WENG Zhixue, HUANG Zhiming, et al. PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)*[J]. 1991, 9(3): 238-245.DOI:
PHASE EQUILIBRIUM FOR THE TERNARY SYSTEM VINYL CHLORIDE-CHLORINATED POLYETHYLENE-POLY(VINYL CHLORIDE)*
<正> Swelling capacity of vinyl chloride (VC) in chlorinated polyethylene (CPE) with 25—40 wt% Cl at temperature 30—57℃was studied and their relationships were correlated with Langmuir and Freundlich adsorption equations. A ternary phase diagram for VC-CPE-PVC was also established. In-situ polymerization conditions of CPE-g-VC were proposed and CPE content control was analyzed for the manufacturing process of CPE-g-VC graft product based on results of phase equilibrium study.
Abstract
Swelling capacity of vinyl chloride (VC) in chlorinated polyethylene (CPE) with 25—40 wt% Cl at temperature 30—57℃ was studied and their relationships were correlated with Langmuir and Freundlich adsorption equations. A ternary phase diagram for VC-CPE-PVC was also established. In-situ polymerization conditions of CPE-g-VC were proposed and CPE content control was analyzed for the manufacturing process of CPE-g-VC graft product based on results of phase equilibrium study.