SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER
Note|Updated:2021-06-21
|
SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER
SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER
高分子科学(英文版)2008年26卷第1期 页码:117-119
Affiliations:
Author bio:
Funds:
DOI:
中图分类号:
Scan for full text
Tao Xu, Wei Yuan, Shen-jun Wang, 等. SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER[J]. 高分子科学(英文版), 2008,26(1):117-119.
Tao Xu, Wei Yuan, Shen-jun Wang, et al. SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER[J]. 2008,26(1):117-119.
Tao Xu, Wei Yuan, Shen-jun Wang, 等. SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER[J]. 高分子科学(英文版), 2008,26(1):117-119.DOI:
Tao Xu, Wei Yuan, Shen-jun Wang, et al. SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER[J]. 2008,26(1):117-119.DOI:
SYNTHESIS OF POLYURETHANE MODIFIED BISMALEIMIDE (UBMI) AND POLYURETHANE-IMIDE ELASTOMER
Urethane modified bismaleimide (UBMI) was synthesized by the reaction of maleic anhydride (MA) with NCO group terminated polyurethane prepolymer (PUP) in presence of acetone. The product was determined by infrared analysis. Then ultrasonic assistant process was introduced into the solvent removal of the prepolymer mixture of UBMI and PUP. Polyurethane-imide (PUI) elastomer was synthesized from the above PUP-UBMI prepolymer mixture by the infusion technology with 2,5-dimethyl-2,5-bis(tert-butylperoxy)-hexane (B25) as liquid initiator at 120°C. The thermal properties and stress-strain behavior of PUI elastomer was characterised by thermogravimetric (TG) analysis and tensile testing apparatus, respectively. Compared with pure polyurethane elastomer, the PUI elastomer composite showed the better thermal stability.
Abstract
Urethane modified bismaleimide (UBMI) was synthesized by the reaction of maleic anhydride (MA) with NCO group terminated polyurethane prepolymer (PUP) in presence of acetone. The product was determined by infrared analysis. Then ultrasonic assistant process was introduced into the solvent removal of the prepolymer mixture of UBMI and PUP. Polyurethane-imide (PUI) elastomer was synthesized from the above PUP-UBMI prepolymer mixture by the infusion technology with 2,5-dimethyl-2,5-bis(tert-butylperoxy)-hexane (B25) as liquid initiator at 120°C. The thermal properties and stress-strain behavior of PUI elastomer was characterised by thermogravimetric (TG) analysis and tensile testing apparatus, respectively. Compared with pure polyurethane elastomer, the PUI elastomer composite showed the better thermal stability.