Morphology Evolution, Conductive and Viscoelastic Behaviors of Chemically Reduced Graphene Oxide Filled Poly(methyl methacrylate)/Poly(styrene-co-acrylonitrile) Nanocomposites during Annealing
PAPER|Updated:2021-06-21
|
Morphology Evolution, Conductive and Viscoelastic Behaviors of Chemically Reduced Graphene Oxide Filled Poly(methyl methacrylate)/Poly(styrene-co-acrylonitrile) Nanocomposites during Annealing
Chinese Journal of Polymer ScienceVol. 33, Issue 8, Pages: 1162-1175(2015)
Affiliations:
MOE Key Laboratory of Macromolecule Synthesis and Functionalization, Ministry of Education, Department of Polymer Science and Engineering, Zhejiang University, Hangzhou 310027, China
Chao-ying Lin, Min Zuo, Hui-hui Li, et al. Morphology Evolution, Conductive and Viscoelastic Behaviors of Chemically Reduced Graphene Oxide Filled Poly(methyl methacrylate)/Poly(styrene-co-acrylonitrile) Nanocomposites during Annealing[J]. Chinese Journal of Polymer Science, 2015, 33(8): 1162-1175. DOI: 10.1007/s10118-015-1666-3.
DOI:
Chao-ying Lin, Min Zuo, Hui-hui Li, et al. Morphology Evolution, Conductive and Viscoelastic Behaviors of Chemically Reduced Graphene Oxide Filled Poly(methyl methacrylate)/Poly(styrene-co-acrylonitrile) Nanocomposites during Annealing[J]. Chinese Journal of Polymer Science, 2015, 33(8): 1162-1175. DOI: 10.1007/s10118-015-1666-3.DOI:
Morphology Evolution, Conductive and Viscoelastic Behaviors of Chemically Reduced Graphene Oxide Filled Poly(methyl methacrylate)/Poly(styrene-co-acrylonitrile) Nanocomposites during Annealing
The effect of chemically reduced graphene oxide (CRGO) on the phase separation behavior of poly(methyl methacrylate)/poly(styrene-
co
-acrylonitrile) (PMMA/SAN) blends and the simultaneous response of rheological and conductive behavior of PMMA/SAN/CRGO nanocomposites upon annealing above the phase-separation temperatures were investigated. The introduction of CRGO causes the decrease of binodal temperature and the increase of spinodal temperature for PMMA/SAN blends and then enlarges their metastable regime. During annealing
the well-dispersed CRGO in the homogeneous blend matrix tends to be selectively located in the SAN-rich phase with the evolution of phase separation and then the CRGO further agglomerates effectively in the SAN-rich phase to form the conductive pathway. Thermal-induced dynamic percolation is observed for both the resistivity
ρ
and dynamic storage modulus
G
' as a function of annealing time. The resistivity variation is ascribed to the agglomeration of CRGO in the SAN-rich phase
while the modulus evolution is attributed to the combined contribution of phase separation for blend matrix and the agglomeration of CRGO in the SAN-rich phase.