The asymmetric polyamide-6 (PA6) membranes were prepared by thermally induced phase separation. From the scanning electron microscopy (SEM) images
it is observed that with the increase of silicon dioxide (SiO2) content the structure of obtained membranes gradually varied from cellular structure to large ball-shaped cluster aggregates. Subsequently
with the addition of SiO2
pure water flux increased first and then decreased
while rejection showed the opposite trend. Besides
raising the coagulation bath temperature was favorable to increase pure water flux. Consequently
different membrane morphologies and performance were obtained by changing SiO2 content and coagulation bath temperature.
Abstract
The asymmetric polyamide-6 (PA6) membranes were prepared by thermally induced phase separation. From the scanning electron microscopy (SEM) images
it is observed that with the increase of silicon dioxide (SiO2) content the structure of obtained membranes gradually varied from cellular structure to large ball-shaped cluster aggregates. Subsequently
with the addition of SiO2
pure water flux increased first and then decreased
while rejection showed the opposite trend. Besides
raising the coagulation bath temperature was favorable to increase pure water flux. Consequently
different membrane morphologies and performance were obtained by changing SiO2 content and coagulation bath temperature.