Aromatic copolyamides were synthesized by the Yamazaki phosphorylation method starting from bis(4-carboxyphenyl) phenyl phosphine oxide
terephthalic acid and 4
4'-diaminodiphenyl methane. The copolymers with inherent viscosities of 0.52-0.99 dL/g were obtained. The structures of the copolyamides were characterized by elemental analysis
FTIR and NMR. The glass transition temperatures were measured by DSC and DMA
respectively
and the results showed that the Tgs of the polymers were higher than 287oC. Thermal decomposition temperatures of the copolyamides at 5% weight loss were found in the range of 423-469oC by TGA. Most of the copolymers were readily soluble in a variety of organic solvents such as NMP
DMAc
m-cresol and so on. The tensile experiments of the thin films showed that the polymers had good mechanical properties.
Abstract
Aromatic copolyamides were synthesized by the Yamazaki phosphorylation method starting from bis(4-carboxyphenyl) phenyl phosphine oxide
terephthalic acid and 4
4'-diaminodiphenyl methane. The copolymers with inherent viscosities of 0.52-0.99 dL/g were obtained. The structures of the copolyamides were characterized by elemental analysis
FTIR and NMR. The glass transition temperatures were measured by DSC and DMA
respectively
and the results showed that the Tgs of the polymers were higher than 287oC. Thermal decomposition temperatures of the copolyamides at 5% weight loss were found in the range of 423-469oC by TGA. Most of the copolymers were readily soluble in a variety of organic solvents such as NMP
DMAc
m-cresol and so on. The tensile experiments of the thin films showed that the polymers had good mechanical properties.