The direct polymerization of an unsymmetrical kink non-coplanar heterocyclic diamine (1) with various aromatic bis(trimellitimide)s (2a-e) using triphenyl phosphite and pyridine as condensing agents could generate a series of new aromatic poly(amide imide)s (3a-e) containing the kink non-coplanar phthalazinone heterocyclic units in the polymer main chains with inherent viscosities of 0.58-0.66 dL/g. The polymers are readily soluble in a variety of solvents such as N
N-dimethylformamide
N
N-dimethylacetamide
dimethyl sulfoxide
N-methyl-2-pyrrolidinone
pyridine and m-cresol and can be cast to form flexible and tough films. The glass transition temperatures of polymers (Tg) are in the range of 301-327℃
and the temperatures for 5% weight loss in nitrogen are in the range of 498-521 ℃.
Abstract
The direct polymerization of an unsymmetrical kink non-coplanar heterocyclic diamine (1) with various aromatic bis(trimellitimide)s (2a-e) using triphenyl phosphite and pyridine as condensing agents could generate a series of new aromatic poly(amide imide)s (3a-e) containing the kink non-coplanar phthalazinone heterocyclic units in the polymer main chains with inherent viscosities of 0.58-0.66 dL/g. The polymers are readily soluble in a variety of solvents such as N
N-dimethylformamide
N
N-dimethylacetamide
dimethyl sulfoxide
N-methyl-2-pyrrolidinone
pyridine and m-cresol and can be cast to form flexible and tough films. The glass transition temperatures of polymers (Tg) are in the range of 301-327℃
and the temperatures for 5% weight loss in nitrogen are in the range of 498-521 ℃.
关键词
Keywords
references
The trial reading is over, you can activate your VIP account to continue reading.