By using a two-stage soapless emulsion polymerization
four kinds of core-shell nanoparticles have been prepared
which are composed of a polystyrene core having an average diameter of 256 nm and a poly(methyl methacrylate-co-acrylicacid) shell. The transmission electron microscopy (TEM) micrographs and the atomic force microscopy (AFM) imagesevidenced the presence of a core-shell structure. In the infrared spectra
the shift of vCOOH to lower wavenumber withincreasing Eu3+ ion content indicates that coordination between the oxygen of the carboxylic group and Eu3+ has occurred.The fluorescence intensity of 5D0-7F2 transition was observed to reach its maximum with a carboxyl group molar percentage of 40% in the shell and an Eu3+/—COO- molar ratio of 1:3.The fluorescence intensity ratio of 5D0-7F2 to 5D0-7F1 transition reached its maximum with an Eu3+/—COO- molar ratio of 1:3 for all the four series.
Abstract
By using a two-stage soapless emulsion polymerization
four kinds of core-shell nanoparticles have been prepared
which are composed of a polystyrene core having an average diameter of 256 nm and a poly(methyl methacrylate-co-acrylicacid) shell. The transmission electron microscopy (TEM) micrographs and the atomic force microscopy (AFM) imagesevidenced the presence of a core-shell structure. In the infrared spectra
the shift of vCOOH to lower wavenumber withincreasing Eu3+ ion content indicates that coordination between the oxygen of the carboxylic group and Eu3+ has occurred.The fluorescence intensity of 5D0-7F2 transition was observed to reach its maximum with a carboxyl group molar percentage of 40% in the shell and an Eu3+/—COO- molar ratio of 1:3.The fluorescence intensity ratio of 5D0-7F2 to 5D0-7F1 transition reached its maximum with an Eu3+/—COO- molar ratio of 1:3 for all the four series.