TRANSESTERIFICATION IN POLYPHENYLSILSISQUIOXANE (PPSQ)/POLY ETHYLENE TEREPHTHALATE (PET) BLENDS*
Papers|Updated:2021-06-21
|
TRANSESTERIFICATION IN POLYPHENYLSILSISQUIOXANE (PPSQ)/POLY ETHYLENE TEREPHTHALATE (PET) BLENDS*
Vol. 13, Issue 4, Pages: 366-374(1995)
Affiliations:
1. Polymer Physics Laboratory
2. Institute of Chemistry
3. Academia Sinica
4. Beijing Present Address: Department of Chemistry ,100080
5. Shandong University
6. Jinan 250100
7. Beijing 100080
Author bio:
Funds:
DOI:
CLC:O631
Published:20 December 1995
Accepted:
Scan QR Code
[1]李桂芝,施良和,叶美玲,赵春田,徐懋.TRANSESTERIFICATION IN POLYPHENYLSILSISQUIOXANE(PPSQ)/POLY ETHYLENE TEREPHTHALATE (PET) BLENDS[J].Chinese Journal of Polymer Science,1995,{4}(04):366-374.
LI Guizhi, SHI Lianghe, YE Meiling, et al. TRANSESTERIFICATION IN POLYPHENYLSILSISQUIOXANE (PPSQ)/POLY ETHYLENE TEREPHTHALATE (PET) BLENDS*[J]. 1995, 13(4): 366-374.
[1]李桂芝,施良和,叶美玲,赵春田,徐懋.TRANSESTERIFICATION IN POLYPHENYLSILSISQUIOXANE(PPSQ)/POLY ETHYLENE TEREPHTHALATE (PET) BLENDS[J].Chinese Journal of Polymer Science,1995,{4}(04):366-374.DOI:
LI Guizhi, SHI Lianghe, YE Meiling, et al. TRANSESTERIFICATION IN POLYPHENYLSILSISQUIOXANE (PPSQ)/POLY ETHYLENE TEREPHTHALATE (PET) BLENDS*[J]. 1995, 13(4): 366-374.DOI:
TRANSESTERIFICATION IN POLYPHENYLSILSISQUIOXANE (PPSQ)/POLY ETHYLENE TEREPHTHALATE (PET) BLENDS*
The chemical structure of copolymer formed in the transesterification of PPSQ/PET blendsduring melt-processing is deduced from the
1
H-NMR spectra. The transesterification extent ofthis blend is interpreted by the changes of crystalline melting peak in DSC thermograms of the in-soluble products containing unreacted PET and some block PPSQ segments. Effects of composi-tion of blend ladderlike regularity of PPSQ on the reaction extent have also been discussed.Inclusion of some block PPSQ segments in PET has no influence on the crystalline morphology ofPET.
Abstract
The chemical structure of copolymer formed in the transesterification of PPSQ/PET blendsduring melt-processing is deduced from the
1
H-NMR spectra. The transesterification extent ofthis blend is interpreted by the changes of crystalline melting peak in DSC thermograms of the in-soluble products containing unreacted PET and some block PPSQ segments. Effects of composi-tion of blend ladderlike regularity of PPSQ on the reaction extent have also been discussed.Inclusion of some block PPSQ segments in PET has no influence on the crystalline morphology ofPET.
关键词
Keywords
references
The trial reading is over, you can activate your VIP account to continue reading.
Multiple-Responsive Chiral Hydrogels from Helical Dendronized Poly(phenylacetylene)s
End-group and Side-chain Dual-engineering of Selenium-fused Acceptors for 20.08% Efficiency Polymer Solar Cells with Low Energy Loss
2026-9 Contents
Pyrimidoisoindigo-based Polymers for Ambipolar Charge Transport
Upgrading Commercially Available Polyethylene to High-value Materials with Strong Mechanical Performance and Hydrophilicity by Blending with Ethylene/meta-Methoxystyrene Copolymers