SYNTHESIS AND FREE RADICAL POLYMERIZATION OF 2-OXO-3-METHYLEN E-5-PHENYL-1,4-DIOXAN
Papers|Updated:2021-06-21
|
SYNTHESIS AND FREE RADICAL POLYMERIZATION OF 2-OXO-3-METHYLEN E-5-PHENYL-1,4-DIOXAN
Vol. 11, Issue 2, Pages: 153-157(1993)
Affiliations:
1. Chemistry Department, Graduate School, Academia Sinica,Beijing,100039
2. Graduate School
3. Academia Sinica
4. Beijing
5. 100039
Author bio:
Funds:
DOI:
CLC:
Published:20 June 1993
Accepted:
Scan QR Code
[1]冯品珍.SYNTHESIS AND FREE RADICAL POLYMERIZATION OF 2-OXO-3-METHYLEN E-5-PHENYL-1,4-DIOXAN[J].Chinese Journal of Polymer Science,1993,{4}(02):153-157.
FENG Pinzhen. SYNTHESIS AND FREE RADICAL POLYMERIZATION OF 2-OXO-3-METHYLEN E-5-PHENYL-1,4-DIOXAN[J]. 1993, 11(2): 153-157.
[1]冯品珍.SYNTHESIS AND FREE RADICAL POLYMERIZATION OF 2-OXO-3-METHYLEN E-5-PHENYL-1,4-DIOXAN[J].Chinese Journal of Polymer Science,1993,{4}(02):153-157.DOI:
FENG Pinzhen. SYNTHESIS AND FREE RADICAL POLYMERIZATION OF 2-OXO-3-METHYLEN E-5-PHENYL-1,4-DIOXAN[J]. 1993, 11(2): 153-157.DOI:
SYNTHESIS AND FREE RADICAL POLYMERIZATION OF 2-OXO-3-METHYLEN E-5-PHENYL-1,4-DIOXAN
was synthesized by a set of reactions. Several intermediates were prepared and characterized in order to determine the monomer structure. The presence of chiral centers in the intermediates and resulting monomer makes it complicated to separate
purify and characterize them. It is a very reactive monomer which will polymerize even at room temperature if expose to moisture and air. This monomer can undergo essentially quantitative flee radical ring opening polymerization. The driving force for ring opening is the formation of new carbonyl group and benzylic radical. The monomer and polymer structure were established by IR
1
H NMR
13
C NMR and elemental analysis or high resolution mass spectrum. The molecular weight of the resulting polymer was estimated by viscosity determination.
Abstract
The novel cyclic monomer
2-oxo-3-methylene-5-phenyl-1
4-dioxan
was synthesized by a set of reactions. Several intermediates were prepared and characterized in order to determine the monomer structure. The presence of chiral centers in the intermediates and resulting monomer makes it complicated to separate
purify and characterize them. It is a very reactive monomer which will polymerize even at room temperature if expose to moisture and air. This monomer can undergo essentially quantitative flee radical ring opening polymerization. The driving force for ring opening is the formation of new carbonyl group and benzylic radical. The monomer and polymer structure were established by IR
1
H NMR
13
C NMR and elemental analysis or high resolution mass spectrum. The molecular weight of the resulting polymer was estimated by viscosity determination.