<正> The infrared emissivity of conducting polymers in 8—20μm and at 50—150℃in the direction of normal line has been measured as a function of wavelength
conductivity at room temperature
counterion
doping levels
measuring temperature and thickness of sample.
Abstract
The infrared emissivity of conducting polymers in 8—20μm and at 50—150℃ in the direction of normal line has been measured as a function of wavelength
conductivity at room temperature
counterion
doping levels
measuring temperature and thickness of sample.
关键词
Keywords
references