This paper reports a new method to prepare chitosan membrane which could be used as a biomedical material.Addition of a fixation agent composed of alcohol
glycerol and potassium hydroxide can acceletate the sol-gel transformationprocess and hence shorten the prepedion perod. The present method takes about 6 h to get a flexible membrane with fineappearance. The physical and biological properties of the membrane were also investigated and compared with the membraneprepared by conventional method.
Abstract
This paper reports a new method to prepare chitosan membrane which could be used as a biomedical material.Addition of a fixation agent composed of alcohol
glycerol and potassium hydroxide can acceletate the sol-gel transformationprocess and hence shorten the prepedion perod. The present method takes about 6 h to get a flexible membrane with fineappearance. The physical and biological properties of the membrane were also investigated and compared with the membraneprepared by conventional method.
关键词
Keywords
references
The trial reading is over, you can activate your VIP account to continue reading.